Stopień lepkości ISO | 150 | 220 | 320 | 460 | 680 | 1000 |
Lepkość kin., ASTM D 445 | | | | | | |
cSt w temp. 40ºC | 150 | 220 | 320 | 460 | 680 | 1000 |
cSt w temp. 100º C | 22.2 | 30.4 | 40.6 | 54.1 | 75.5 | 99.4 |
Wskaźnik lepkości ASTM D 2270 | 176 | 180 | 181 | 184 | 192 | 192 |
Temp. płynięcia, [°C], ASTM D 97 | -54 | -45 | -48 | -48 | -42 | -33 |
Temp. zapłonu, [°C], ASTM D 92 | 233 | 233 | 233 | 234 | 234 | 234 |
Brookfield w temp. 0 º F (-18 º C), cP, ASTM D 2983 | | | | | 41000 | 96000 |
Brookfield w temp. -20 º F (-28 º C), cP, ASTM D 2983 | 18200 | 35000 | 57000 | 107000 | 156000 | 500000 |
Gęstość 15 º C, kg/dcm3 | 0.86 | 0.86 | 0.86 | 0.86 | 0.86 | 0.87 |
Całkowita liczba kwasowa, mg KOH/g, ASTM D 664 | 0.9 | 0.9 | 0.9 | 0.9 | 0.9 | 0.9 |
Aparatczterokulowy zacieranie, kG, ASTM D 2783 | | | | | | |
Obciążenie zespawania | 200 | 200 | 200 | 200 | 200 | 200 |
Wskaźnik zużycia | 51 | 51 | 51 | 51 | 51 | 51 |
FZG Micropitting, FVA Proc No. 54, 90°Z | | | | | | |
[stopień] | 10 | 10 | 10 | 10 | 10 | 10 |
GFT- Klasa | Wysoka | Wysoka | Wysoka | Wysoka | Wysoka | Wysoka |
Test FZG, ISO 14635-1 (mod) A/8.3/90, [stopień] | 13 | 14 | 14 | 14 | 14 | 14 |
FZG skrabetest, ISO 14635-1 (mod), A/16,6/90, sammenbrudsniveau | Ikke testet | >14 | >14 | >14 | >14 | >14 |
Korozja miedzi 3 h, w temp. 121 ºC, ASTM D 130 | 1B | 1B | 1B | 1B | 1B | 1B |
Test FZG, ISO 14635-1 (mod) A/16.6/90, [stopień] | Spełnia | Spełnia | Spełnia | Spełnia | Spełnia | Spełnia |
Deemulgacja olejów EP, woda niezwiązana, ml, ASTM D 2711 | 88 | 87 | 85 | 84 | 87 | |
Oddzielanie wody, ASTM D 1401, czas do 40/37/3 w temp. 82º C, minuty | 10 | 10 | 10 | 15 | 25 | 40 |
ASTM D 892, sekw. II, ml/ml | 0/0 | 0/0 | 0/0 | 20/0 | 0/0 | 0/0 |